View Single Post
Old 03-10-2013, 11:45 AM
rhodeisland rhodeisland is offline
Motorized Bicycle Senior Member
Join Date: Oct 2012
Location: Rhode Island
Posts: 83
Default Re: Paint Disaster, Any Clues?

The previous coats did not flash off enough so the solvents in the later coats broke the skin and it slid.
I used two component epoxy when I fair out components but that would not be cost effective for one tank.
I would give the primer more flash times between coats the more the better because it will shrink in and also sand much easier with better results.
Welcome to the world of painting.
Reply With Quote