in this picture i mixed some salt vineger and hydrogen peroxide like i told you before . now i'm useing brass so you can see whats happening. copper nickle zink brass .but for this i chose brass you so you can see anyways in this picture i have the brass on the positive and the nail as my negative now my connection to the brass is above the vinager line because if its below the vieger line it will eat your connection the darker bottle the the finished solution